This website uses cookies

We use cookies to enhance your experience and support COUNTER Metrics for transparent reporting of readership statistics. Cookie data is not sold to third parties or used for marketing purposes.

Skip to main content
null
Journal of Microelectronics & Elect Pkg
  • Menu
  • Articles
    • General
    • Technical Article
    • All
  • For Authors
  • Editorial Board
  • About
  • Issues
  • IMAPSource Proceedings
  • search
  • LinkedIn (opens in a new tab)
  • RSS feed (opens a modal with a link to feed)

RSS Feed

Enter the URL below into your favorite RSS reader.

http://localhost:47198/feed
ISSN 1551-4897
General
Vol. 15, Issue 2, 2018April 01, 2018 EDT

Characterization of Mechanical Properties and Creep Behavior of Woven Glass/Epoxy Substrates by Nanoindentation

Abel Misrak, Luu Nguyen, Steven Kummerl, Dereje Agonafer,
Nanoindentationprinted circuit boardsreliabilityatomic force microscopyviscoelasticitycreep test
Copyright Logoccby-nc-nd-4.0 • https://doi.org/10.4071/imaps.654387

Articles in Vol. 15, Issue 2, 2018

Vol. 15, Issue 2, 2018
  • Equivalent Capacitance Approach to Calculate Effective Roughness Dielectric Parameters for Copper Foils on Printed Circuit Boards
    Marina Y. KoledintsevaTracey Vincent
  • Low Temperature Cofiring and Dielectric Properties of Ca-Doped Al2O3/K2O3–B2O3–SiO2 Composite Ceramics for LTCC Applications
    Zhe SongJoanna ChuKun HuangLasse NorénZhenxiao FuYun Liu
  • LTCC-Based Highly Integrated SiPM Module with Integrated Liquid Cooling Channels for High Resolution Molecular Imaging
    Rainer DohleIlaria SaccoThomas RittwegThomas FriedrichGerold HenningJörg GoßlerPeter Fischer
  • Characterization of Mechanical Properties and Creep Behavior of Woven Glass/Epoxy Substrates by Nanoindentation
    Abel MisrakLuu NguyenSteven KummerlDereje Agonafer
  • Thermal Interface Materials and Cooling Technologies in Microelectronic Packaging—A Critical Review
    Dinesh P. R. ThanuBoxi LiuMarco Aurelio Cartas
  • Dark Current Leakage in Optoelectronic Hermetic Packages
    Clara DionetGoran PerosevicJeff JavierSammie FernandezTaylor HurdleMaziar MoradiAndrew NeelyKevin MaMarwan Albarghouti
Journal of Microelectronics & Elect Pkg
Misrak, Abel, Luu Nguyen, Steven Kummerl, and Dereje Agonafer. 2018. “Characterization of Mechanical Properties and Creep Behavior of Woven Glass/Epoxy Substrates by Nanoindentation.” Journal of Microelectronics and Electronic Packaging 15 (2): 95–100. https://doi.org/10.4071/imaps.654387.